Tuesday, April 19, 2016

Re: [MW:24722] orifice flange nipple seal welding & PT before hydro or after hydro hydro ?

If you have already welded the nipple after hydro test, go for re-hydro.

Thanks

On Fri, Apr 1, 2016 at 5:26 PM, Amul Raj <win.amul@gmail.com> wrote:

 

 Dear Experts,


Our piping team prepared the orifice flange nipple seal welding & PT after hydro test

But, our client wants to install the nipple & seal weld before hydro test   

Which is the right method?

 

Regards,

Amul Raj T

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/501913ef-9fd0-4f55-8675-d2dfe74a6d0d%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAK2QV3TgBzQvBWNxgq4VpiDr%2B1hkv1npe-S3g0E_uGo5ZahCPw%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...