There's no answer to such questions in these "Open Forum". If such conditions are stipulated in your project specifications, then it's deemed as mandatory. In order  to get a deviation or any waiver please discuss the same with clients and then come up with some consent/understanding.

 

Many clients insists on "Dehydrogenation" to safeguard against hydrogen induced damages (especially wet hydrogen cracking") in refining environments. In view of such imminent damage and other forms of hydrogen damages in refining environments, dehydrogenation treatment is most commonly asked for in present day fabrication standards.

 

Thanks.

 

Pradip Goswami, P.Eng,IWE
Independent Welding & Metallurgical Engineering Specialist & Consultant.
Ontario,Canada.
ca.linkedin.com/pub/pradip-goswami/5/985/299

pgoswami@quickclic.net

pradip.goswami@gmail.com

 

 


From: 'Neilashkumar' via Materials & Welding [mailto:materials-welding@googlegroups.com]
Sent: Thursday, April 07, 2016 1:30 AM
To: materials-welding@googlegroups.com; Jim Price
Subject: [MW:24643] Intermediate stress relief treatment

 

 

 

Dear All, 



Good Day ! As per our client aramco , insisting us to do dehydrogenation treatment for P11 material after welding completion for four hours prior to PWHT.



Please clarify whether post heat maintainence for 4hours is mandatory for fillet weld.



As per our WPS  I am doing it for  groove joints , it is clad vessel for 145 inch diameter ... 



Above that insulation and pad welding Accor , is there any clause given in ASME section states that post heat maintainence is not required for P11 material.





As per aramco standard SAESW014 General it is given

 


P.NEILASHKUMAR 

Sent from my iPad

MOB : 966 551094590

            + 91 9952110791

 

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/0B59ABE0-AA41-4BD5-9389-F1AF70590CAB%40yahoo.com.
For more options, visit https://groups.google.com/d/optout.

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/!%26!AAAAAAAAAAAYAAAAAAAAAOT5XfyRhstKvyeqQRSrfFXCgAAAEAAAAN8IATtSA6xDg3KrvkrY%2BRkBAAAAAA%3D%3D%40quickclic.net.
For more options, visit https://groups.google.com/d/optout.

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAK%3Dnts06j0vtf%2Bfccvc6iBasCDhRx6aCPxGJ73iBXuDW-dXSeA%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...