Re: [MW:24665] Run-Out Length for SMAW Process

Run out length is the time to do a length of weld in a certain length of time, e.g. If a welder welded a 2 inches of weld in 1 minute, then your run out length is 2 inch per minute. Just time your welder from when he starts his weld to the time he stops, then measure how long his weld is.

On Saturday, 9 April 2016, Kurniatullah Sirajudin <kurniatullahsirajudin@gmail.com> wrote:
Dear Expert,

A week ago, i received comment regarding welding for smaw process.

My client ask to me, run-out length for smaw process.

I don't know what is run-out length.


Please advise me 


Thank you & Regards

Kurniatullah Sirajudin

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/bb9ef69c-8c36-42e8-b090-7dd6d32d8af3%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAGta9%3DtiS%2BoKRm%2BtNFiz7%2BYMSBjyQnNZsBaQxgd7MCxN_eec6A%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...