Dear Experts,

Regarding fillet size minimum 70% of less thickness plate to be
considered.... And regarding plate qualification you have to just
conform as per drawing which plate material you are going top weld. If
it is mild steel then you can qualify IS 2062

Thanks,
Balamurugan,
L&T

On 4/13/16, 'prem_nautiyal26' via Materials & Welding
<materials-welding@googlegroups.com> wrote:
> Hi
> You have to refer approved construction drawing for the required fillet
> size.
> Else you may refer the construction code.
> If it is B 31. 3 then you may please use a 6mm size fillet.
>
> Regards
>
> Prem Nautiyal
>
>
>
> Sent from Samsung Mobile
>
> <div>-------- Original message --------</div><div>From: Vivek Pandey
> <vivek.pande06@gmail.com> </div><div>Date:12/04/2016 4:08 AM (GMT-05:00)
> </div><div>To: materials-welding@googlegroups.com </div><div>Subject: Re:
> [MW:24673] WQT fillet size </div><div>
> </div>Dear Tushar
> You can conduct fillet weld on pipe to plate as per section IX table
> QW-452.5 for guidence.
> Yes you can use IS2062 plate P-No. and Group No. that is mentioned table
> QW/QB-422 see section IX edition 2013
>
> On 12-Apr-2016 3:56 pm, "Tushar rao" <tushar.areva@gmail.com> wrote:
> Dear Experts,
>
> I want to cunduct fillet on pipe to plate. Pipe thk is 5.54 mm and plate thk
> is 10 mm.
>
> What is fillet size as per sec-9.
>
> And can i used IS 2062 plate in fillet test. Which was not mention in QW 422
> table.
>
> Please give feedback.
>
> Regards
>
> Tushar Rao
>
> --
> http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
> The views expressed/exchnaged in this group are members personel views and
> meant for educational purposes only, Users must take their own decisions
> w.r.t. applicable code/standard/contract documents.
> ---
> You received this message because you are subscribed to the Google Groups
> "Materials & Welding" group.
> To unsubscribe from this group and stop receiving emails from it, send an
> email to materials-welding+unsubscribe@googlegroups.com.
> To post to this group, send email to materials-welding@googlegroups.com.
> To view this discussion on the web visit
> https://groups.google.com/d/msgid/materials-welding/137fa05d-6826-4408-bf0c-94b4db82ad1c%40googlegroups.com.
> For more options, visit https://groups.google.com/d/optout.
> --
> http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
> The views expressed/exchnaged in this group are members personel views and
> meant for educational purposes only, Users must take their own decisions
> w.r.t. applicable code/standard/contract documents.
> ---
> You received this message because you are subscribed to the Google Groups
> "Materials & Welding" group.
> To unsubscribe from this group and stop receiving emails from it, send an
> email to materials-welding+unsubscribe@googlegroups.com.
> To post to this group, send email to materials-welding@googlegroups.com.
> To view this discussion on the web visit
> https://groups.google.com/d/msgid/materials-welding/CANCwoY%3Dmhm68_HGBVFsXTJqWs4-UWmmjWRAL-F9Hgh35fpG3NA%40mail.gmail.com.
> For more options, visit https://groups.google.com/d/optout.
>
> --
> http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
> The views expressed/exchnaged in this group are members personel views and
> meant for educational purposes only, Users must take their own decisions
> w.r.t. applicable code/standard/contract documents.
> ---
> You received this message because you are subscribed to the Google Groups
> "Materials & Welding" group.
> To unsubscribe from this group and stop receiving emails from it, send an
> email to materials-welding+unsubscribe@googlegroups.com.
> To post to this group, send email to materials-welding@googlegroups.com.
> To view this discussion on the web visit
> https://groups.google.com/d/msgid/materials-welding/2doumm4ljomu75toxue7wk93.1460554289063%40email.android.com.
> For more options, visit https://groups.google.com/d/optout.
>

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAL9C6DZ%3DSJtLhQpMcvNLgQRaxYOHes2a%3D4hEy%2B1BO061Htp9Hg%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...

Re: [MW:10788] ON PLOT PIPING & OFF PLOT PIPING

Piping systems involved for the flow lines and gathering lines from the well head isolation valve to the production facility or processing plant isolation valve are determined as OFF PLOT. ON PLOT defines piping system in the processing plant and production platform. ANSI/ASME B31.4 applies for off plot piping system. B31.4 allows the use of either API 1104 or ASME section IX (as appropriate). However, occasionally, a very small system such as piping within 500 feet of a processing plant (some client also said 400 feet) may be declared B31.3 rather than B31.4. When B31.3 is invoked, only ASME Section IX is used. before you decide which code to use for welding procedure and/or welder qualification for pipe welding, you have to know the design and construction code applicable to the system. Please read far enough into scope and diagram illustrating the application of either B31.3 and B31.4 hope this helps rgds 2011/4/21 pradip kumar sil < pradipsil@gmail.com > Dear all, ...