Dear Experts,

We are doing pipeline  project for international client at UAE. We have completed around 400 joints(10 inch-11.1 mm) at site on conditional PQR( Except SSC/SOHIC  testing) as per NACE MR-0175/ISO 15156

Now the PQR test conducted for the SSC test and SOHIC test.

But the test lab informed that linear indication was observed in two test specimen after 30 days SSC test.

Now the client instructed to go more etching the surface and macroscopic examination.

Please suggest any acceptance criteria and resolution. Failure of the test will result huge impact on the 400 welded joints. Please suggest.

Pipeline Material:API 5L Gr.B X-60 as per shell standards.


Kalemullah
UAE-0569902364
 

Get your own FREE website, FREE domain & FREE mobile app with Company email.  
Know More >

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/20160413160528.13286.qmail%40f4mail-235-76.rediffmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35633] IP Joint

Hello experts, I would like to know what is IP joints in piping(31.3)?  Regards Saurabh -- https://materials-welding.blogspot.com/...