Thursday, April 7, 2016

[MW:24651] Carbon/Manganese pressure vessel ASME VIII, Crack after PWHT

Whts exactly joint geometry?
top and bottom bevel thk?

is it equal??

or unequal??

whts filer metal??

is joint well supported from both end??

did u used crushed flux??

flux was preheated??

How you hve filled groove top full complete after other side..??


--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/c94adad2-7120-423f-90db-cf0935ba9e1d%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...