Monday, April 18, 2016

Re: [MW:24715] Re: GTAW weld weaving

Hi!
As such no code address about weaving but emphasis on heat in put
I) Excessive weaving increases heat input Good
ii) Good welding practices suggest about min weaving to reduce heat input viz about 2-3 time the electrode dia
Still  in spite of more weaving, if you can achieve good impact value No problem  and no body should object However experience says it is difficult to achieve consistence Impact result with excessive weaving
Regards
Hegde



On Sunday, 17 April 2016 8:37 PM, Vishwas Keskar Welding Manager Pune India <vvkeskar123@gmail.com> wrote:


ASME SEC IX is lenient on weaving.WPS will guide this . Put the maximum weaving width  in WPS . With 2.4 dia , filler wire , a width of @12 mm is an acceptable width    

On Thursday, March 31, 2016 at 5:00:12 PM UTC+5:30, simon lawrence wrote:
Pls confirm that Weld weaving width ,  weld weave maximum how much we can accepted in GTAW process ?
--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/467d2395-a259-4815-b8db-585cde441a74%40googlegroups.com?utm_medium=email&utm_source=footer.



For more options, visit https://groups.google.com/d/optout.


No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...