Hi,

If Api rp 582 applicable then, impact test is required to qualify weld metal 
BR
Savad

On Saturday, 12 March 2016, Praphulla Phirke <praphulla.dp@gmail.com> wrote:
Dear All
Need your expert opinion on below query.

We are working on new project with Pressure Parts proposed to customer in ASME A335 P11 materials.

Since the ambient temperature is -48C, we need to perform the Impact Test for the same.

We think that the pipe material can be impact tested. Since this test is not a standard requirement for SA335 P11 pipes no guarantee is provided on the resulting minimum impact energy.

Any suggestions ????


Warm Regards
Praphulla

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/BD225BFF-3C90-4F63-9E1D-8ADCD6FD5928%40gmail.com.
For more options, visit https://groups.google.com/d/optout.


--
Withe Best regards

Savad Salahudeen


--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAByzCuHsXtbPAu5var3VK5P5bTOTExt2eC3o%2BBNUADSrW5Azyg%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35633] IP Joint

Hello experts, I would like to know what is IP joints in piping(31.3)?  Regards Saurabh -- https://materials-welding.blogspot.com/...