RE: [MW:22328] Compare Argon with Nitrogen as Purging gas for Super duplex stainless steels

Nitrogen  have multi purpose  at welding  DSS and SDSS 

1- austenitic stabilizer element.
2- delay segma phase which destroy corrosion resistance of material.
3- increase pitting corrosion resistance.

***** you must know that formation of duplex is thermo mechanical process; at welding there are only thermo process so nitrogen is very important element to form austenite and remain the percentage of two phases (( ferrite  and austinite))

On 23 Nov 2014 03:10, "pgoswami" <pgoswami@quickclic.net> wrote:
Hi Nassef,
 
Please see the attachment for additional guidance.A change of backing gas is an essential variable for procedure qualification on DSS/SDSSs(QW-408).
 
Both Ar,or Ar+ N2 or N2+H2(formier gas) are well proven as  backing gas while welding these steels. Presence of Nitrogen containing backing gases are advisable to protect the root from unfavorable austenite/ferrite ratio.This is critical if there's a requirement of ASTM G-48A pitting corrosion test (typically 25 Deg C  for DSS and  35 DegC and above  for SDSS).
 
In absence of the above pitting corrosion tests  pure (100%) Argon may also be used for backing.
 
Thanks.
 
Pradip Goswami, P.Eng,IWE
Welding & Metallurgical Specialist
Ontario, Canada
 


From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Naasief Navsa
Sent: Thursday, November 20, 2014 4:33 AM
To: materials-welding@googlegroups.com
Subject: RE: [MW:22307] Compare Argon with Nitrogen as Purging gas for Super duplex stainless steels

Hi Ahmed,

 

Thank you (Shukran) for the valuable information. One more question, this mix of argon and nitrogen, what ratio's would be optimum.

 

We are Tig welding material that is 0.15mm thick. We typically weld with about 18A, and a linear speed of 50mm/sec. At this point in time we are purging with 100% Argon.

 

Regards,

 

Naasief

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Ahmad el-sharkawy
Sent: 20 November 2014 09:21 AM
To: materials-welding@googlegroups.com
Subject: Re: [MW:22304] Compare Argon with Nitrogen as Purging gas for Super duplex stainless steels

 



On Wed, Nov 19, 2014 at 11:13 PM, Ahmad el-sharkawy <ahmad.sharkawy88@gmail.com> wrote:

dear Noe Mota mixture of argon and nitrogen is the best gas purging for welding duplex and super duplex stainless steel


 

 







On Wed, Nov 19, 2014 at 10:34 PM, Ahmad el-sharkawy <ahmad.sharkawy88@gmail.com> wrote:

dear Naasief Navsa use mix of argon and nitrogen and use low heat input.

 




--

WITH MY BEST WISHES

AHMED ELSHARKAWY
QA/QC ENGINEER
DIPLOMA DEGREE IN WELDING ENGINEERING.
CERTIFIED WELDING INSPECTOR " CWI "
14072901.
ASNT LEVEL II "
RT&VT&UT&PT&MT"
IRECA CERTIFIED LEAD EDITOR ISO 9001/2008.

PREPARING MASTER DEGREE IN WELDING ENGINEERING.




--

WITH MY BEST WISHES

AHMED ELSHARKAWY
QA/QC ENGINEER
DIPLOMA DEGREE IN WELDING ENGINEERING.
CERTIFIED WELDING INSPECTOR " CWI "
14072901.
ASNT LEVEL II "
RT&VT&UT&PT&MT"
IRECA CERTIFIED LEAD EDITOR ISO 9001/2008.

PREPARING MASTER DEGREE IN WELDING ENGINEERING.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.




This email has been scanned for email related threats and delivered safely by Mimecast.
For more information please visit http://www.mimecast.com

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...