Saturday, November 29, 2014

[MW:22421] RE: 22420] how to realise that the film is D4 or D7 , at the timeof film evaluation

Dear friend,
In each 20cm of the film you could see the marking on the film. It's not too much clear and need a little  focus.

From: tugrulhan özdemir
Sent: ‎11/‎29/‎2014 20:59
To: materials-welding@googlegroups.com
Subject: [MW:22420] how to  realise  that the film is D4 or D7  , at the timeof film evaluation

Dear Experts


Is there any way to understand that the film    under review is D4 or D7 ? , at the time of evaluation.

Note: Agfa roll pack films



Regards


Tugrulhan

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...