Re: [MW:22400] G type consumable

A -G consumable does not meet any particular ASME/AWS SFA/A-5.x classification chemistry.  This does not mean that it will not meet a Section IX A-Number chemistry range.  You would need to evaluate the filler metal manufacturer's specified chemistry range to see if it fits one of the A-number chemistry ranges.  Alternatively, you can specificy that the filler metal must meet a certain range.  While not a G filler metal, I typically specify that ER70S-6 must meet the A-Number 1 chemistry requirements.


From: materials-welding@googlegroups.com <materials-welding@googlegroups.com> on behalf of Pravin Poornachandran <htcispravin@gmail.com>
Sent: Friday, November 28, 2014 5:58 AM
To: materials-welding@googlegroups.com
Subject: [MW:22396] G type consumable
 

Dear expert,

Is it true that all G type consumable example ER70S-G don't have A number under ASME?

This group only have F number? Is it true?

Kindly advice.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...