Dear Ahmed,
You must be welding on a base thickness between 16 mm to 25 mm with a clad thickness of to 4 mm. You must be carrying out CuSo4 test to ensure the clad restoration area is free from 825 deposits. Now in doing all this the edge portion where you have your clad interface shall be given a bow shape configuration instead of square edge. When using GMAW process using spray or globular the square edge corner does not get fussed and you will get incomplete fussion all through out the seam. So please change the sequence of de-cladding and get that joint bow shape.
Regards,
Nitin
On Thu, Nov 27, 2014 at 11:29 PM, <george.dilintas@gr.bureauveritas.com> wrote:
Use run-on, run-off plates
best regards
Dr. Georgios Dilintas
Authorized Nuclear Inspector
Authorized Inspector Supervisor
I&F REGIONAL TECHNICAL MANAGER
BUREAU VERITAS HELLAS
Tel: +30 210 40 63 113/4
Fax: +30 210 40 63 118
Cell: +30 69 44 64 62 04
(See attached file: Dilintas_George.vcf)israr ahmed ---27/11/2014 10:27:28---Dear Friend I am using GMAW process for Weld Overlay on Carbon+Alloy 825 Cladded Plate.
From: israr ahmed <ahmedisrar.nm@gmail.com>
To: materials-welding@googlegroups.com
Date: 27/11/2014 10:27
Subject: [MW:22381] Weld Overlay Cladding
Sent by: materials-welding@googlegroups.com
Dear Friend
I am using GMAW process for Weld Overlay on Carbon+Alloy 825 Cladded Plate.
During Cladding process edges of the Cladded Plate Alloy 825 is not fusing properly and during RT its indication Lack of Fusion.
The Feeler Wire Used as SFA 5.4 ER NiCrMo-3
Can any body help me what is the reason.
--
Israr Ahmed Noor Mohammed
+919930308261--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.This message contains confidential information. To know more, please click on the following link: http://disclaimer.bureauveritas.com
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

Comments