see page 196
On Sat, Nov 22, 2014 at 6:10 AM, <sunrock83@gmail.com> wrote:
> thanks for below link. I cant find 9000# although 6000# is mentioned.
>
>
>
> On Friday, November 21, 2014 9:14:55 PM UTC+5:30, Dindo Dela Cruz wrote:
>>
>> follow the link
>>
>> http://www.wmaass.nl/pdfs/catalogue.pdf
>>
>>
>>
>> On Thu, Nov 20, 2014 at 12:00 AM, <sunr...@gmail.com> wrote:
>> > Can somebody help me with Dimensions of 9000# Forged Reducers, Weldoltes
>> > and
>> > Sockolets
>> >
>> > Thanks
>> >
>> > Nilesh Mehta
>> >
>> > --
>> > To post to this group, send email to material...@googlegroups.com
>> > To unsubscribe from this group, send email to
>> > materials-weld...@googlegroups.com
>> > For more options, visit this group's bolg at
>> > http://materials-welding.blogspot.com/
>> >
>> > http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
>> >
>> > The views expressed/exchnaged in this group are members personel views
>> > and
>> > meant for educational purposes only, Users must take their own decisions
>> > w.r.t. applicable code/standard/contract documents.
>> > ---
>> > You received this message because you are subscribed to the Google
>> > Groups
>> > "Materials & Welding" group.
>> > To unsubscribe from this group and stop receiving emails from it, send
>> > an
>> > email to materials-weld...@googlegroups.com.
>> > For more options, visit https://groups.google.com/d/optout.
>
> --
> To post to this group, send email to materials-welding@googlegroups.com
> To unsubscribe from this group, send email to
> materials-welding+unsubscribe@googlegroups.com
> For more options, visit this group's bolg at
> http://materials-welding.blogspot.com/
> http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
>
> The views expressed/exchnaged in this group are members personel views and
> meant for educational purposes only, Users must take their own decisions
> w.r.t. applicable code/standard/contract documents.
> ---
> You received this message because you are subscribed to the Google Groups
> "Materials & Welding" group.
> To unsubscribe from this group and stop receiving emails from it, send an
> email to materials-welding+unsubscribe@googlegroups.com.
> For more options, visit https://groups.google.com/d/optout.
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.
Subscribe to:
Post Comments (Atom)
Re: [MW:35686] HDPE WPS
Refer ASME SEC IX There is separate chapter for Plastic welding . Based on that you have to prepare Sent from my iPhone On 21 Jun 2025, at...
-
Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? ...
-
Definition of buttering from ASME Section IX, QW/QB-492 Definitions: Buttering: the addition of material, by welding, on one or bot...
-
Section I. PRINT READING 3-1. GENERAL a. Drawings . Drawing or sketching is a universal language used to convey all necessary information to...