Dear friend,
Even if any code or standard reference another standard or code like ASME Sec. V, all works should be under your "written practice". Most of standards just push you to have written practice in which you define level of qualifications and their responsibilities and depends on your previous experience.

Regards

From: george.dilintas@gr.bureauveritas.com
Sent: ‎11/‎26/‎2014 15:13
To: materials-welding@googlegroups.com
Subject: Re: [MW:22368] ASME SEC-V , VT requirements for QC Inspector

In Section VIII-1 there is no formal qualification requirement for VT.
Thus, You do not need NDT company to perform VT.
Such a requirement exists in Section B31.1 but with no reference to section V, but again you do not need a NDT company for VT. You may establish an internal qualification scheme for VT in that case.

    best regards

    Dr. Georgios Dilintas

    Authorized Nuclear Inspector
    Authorized Inspector Supervisor


    I&F REGIONAL TECHNICAL MANAGER
    BUREAU VERITAS HELLAS

    Tel: +30 210 40 63 113/4
    Fax: +30 210 40 63 118
    Cell: +30 69 44 64 62 04
    (See attached file: Dilintas_George.vcf)
This message contains confidential information. To know more, please click on the following link: http://disclaimer.bureauveritas.com

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...