Wednesday, November 26, 2014

Re: [MW:22364] ASME SEC-V , VT requirements for QC Inspector

Mr.Veera,
Thank you for your reply and i know this VT requirement.

What i wanted to know is, since i am recently joined here and have only 10 days for fresh and U stamp certification audit,

Can i ask my NDT company procedure and qualify my QC inspector within 5 days with their procedure.

Is it permitted for ASME vessels in Sec V.

Regards
Saravanan

On 26 Nov 2014 16:04, "veera raghava Kommisetti" <kommisetti@gmail.com> wrote:
Unlike other methods, VT can be done my own QC.
just need to write a procedure of your own and qualify your people.
all you need is annual eye exam and basic training.
there is no need for outsourcing VT activities.

On Tue, Nov 25, 2014 at 5:01 PM, Saravanan Sornam <saravanshyla@gmail.com> wrote:

Dear ASME experts,

Please give your suggestions on the following,

As we made contract for VT inspection with our Subconteactor NDT company,
and 1st time we are going to have U stamp Audit for new application after 10 days from now,
I guess it is not reasonable to call VT guy for each inspection in our shop.

NDT Company is 50 kms away from our shop.

So i would like to use NDT company procedure to qualify our own QC inspector to make inspection with ASME AI before we close the final closure in our vessel.
  
Can i make contract with NDT company to give visual inspection training as per ASNT requirement and ammend my QC manual accordingly.

Need your suggestions ASAP.

Regards
Saravanan

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...