Dear Experts,

I am in a situation to establish WPS for in service piping as per 1104 Annex B. The WPS is for a split tee tie in joint (Encirclement Tee)
Split tee ASTM A 516 Grade B
Header pipe 24" sch 60 (API 5L Grade B)

How to select the thickness range ?
How to select dia range ?
What are the essential variables ?

Please guide me to make a preliminary WPS.

Thanks & Regards
Anas Karanath




--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...