Wednesday, November 26, 2014

RE: [MW:22375] Incoloy tube to tube joint welding

Dear friend,
Root cause could be analyzed after you give us some details about the weld.
As I know you did RT previously and didn't see any issue. Also you did PT and same result. It's because of the size of cracks. In which cases that you expect hair like cracks, you should use RT with more definition (x-ray with slow speed films) or a method of PT with more definition (such as fluorescent).

Regards

From: george.dilintas@gr.bureauveritas.com
Sent: ‎11/‎26/‎2014 15:13
To: materials-welding@googlegroups.com
Subject: Re: [MW:22368] Incoloy tube to tube joint welding

Principally RT. What is your thickness?

    best regards

    Dr. Georgios Dilintas

    Authorized Nuclear Inspector
    Authorized Inspector Supervisor


    I&F REGIONAL TECHNICAL MANAGER
    BUREAU VERITAS HELLAS

    Tel: +30 210 40 63 113/4
    Fax: +30 210 40 63 118
    Cell: +30 69 44 64 62 04
    (See attached file: Dilintas_George.vcf)

Inactive hide details for Ranjit Debnath ---25/11/2014 16:14:42---We are welding incoloy tube to tube joint using incoloy filleRanjit Debnath ---25/11/2014 16:14:42---We are welding incoloy tube to tube joint using incoloy filler wire. PQR as per ASME is qualified. P

From: Ranjit Debnath <ranjit.deb87@gmail.com>
To: materials-welding@googlegroups.com
Date: 25/11/2014 16:14
Subject: [MW:22353] Incoloy tube to tube joint welding
Sent by: materials-welding@googlegroups.com





We are welding incoloy tube to tube joint using incoloy filler wire. PQR as per ASME is qualified. PT, RT, hydrotest of joint is acceptable. After bending this tube, when we conducted PT on the weld joint, one surface indication was noticed. This indication disappeared after filing. We cut this joint circumferentially and did micro and macro test. In macro, we found some crack like indication in weld joint.

Can anyone help to analyse and give root cause for this? Which other NDT method we can employ to ensure that all other welded joints do not have these cracks?

--

REGARDS,
RANJIT
Mob:+966532453517
 P Help the environment – please don't print this email unless you really need to!

" Never hate jealous people. They are jealous because they think you are better than them" - By Paulo Coelho

" I always feel happy " You know why? Because I  don't expect anything from anyone!!!. Expectations always hurt. -By Shakespear

"Difficult Roads often leads to beautiful destinations."

" No relationship is all sunshine , but two people can share one umbrella and survive the storm together."

"Some people come in your life as blessings. Some come in your life as lessons."- By Mother Teresa

"Time is free, but  it's priceless. You can't own it, but you can use it. You can't keep it, but you can spend it. Once you've lost it you can never get it back."

"Faith and Prayer both are invisible but they make impossible things Possible! "

" LIFE always offer you a second chance. It's called Tomorrow."

"Be a good person but don't waste time to prove it."

"Don't wait for the perfect moment, take the moment and make it perfect."

" Throw your dreams into space like a kite, and you do not know what it will bring back, a new life, a new friend, a new love, a new country" - By Anais Nin


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at
http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm

The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to
materials-welding+unsubscribe@googlegroups.com.
For more options, visit
https://groups.google.com/d/optout.

This message contains confidential information. To know more, please click on the following link: http://disclaimer.bureauveritas.com

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...