Pravin,
 
Here's some update from Sec-II, Pt-C and Sec-IX on "G" class welding filler metals. In addition to the answers provided below this information will help you to understand the rationale behind "G" type welding consumables.
 
Note,ER-70S-G does not differ much with respect to mechanical properties as compared to respect on the  filler grades in SFA -5.18.
 
As explained below "G" class is specific application base consumable, where the composition, properties are as agreed between the supplier and the purchaser. However if the consumable  falls within the A No range of QW-442, consumable manufacturer may assign the A No to the product(As John Henning had mentioned in his response).
 
 
Thanks.
 
Pradip Goswami, P.Eng,IWE
Welding & Metallurgical Specialist
Ontario, Canada
 

A2.3 “G” Classification:- A2.3.1 This specification includes filler metals classified as ER70S-G [ER48S-G], E70C-G [E48C-G], and E70C-GS [E48C-GS]. The “G” (multiple pass) or “GS” (single pass) indicates that the filler metal is of a “general” classification. It is general because not all of the particular requirements specified for each of the other classifications are specified for this classification. The intent in establishing these classifications is to provide a means by which filler metals that differ in one respect or another (chemical composition, for example) from all other classifications (meaning that the composition of the filler metal, in the case of the example, does not meet the composition specified for any of the classifications in the specification) can still be classified according to the specification.

The purpose is to allow a useful filler metal—ne that otherwise would have to await a revision of the specification —to be classified immediately under the existing specification. This means, then, that two filler metals, each bearing the same “G” classification, may be quite different in some particular respect (chemical composition, again, for example).

 
 
 
ASME Sec-IX
 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of george.dilintas@gr.bureauveritas.com
Sent: Saturday, November 29, 2014 3:19 PM
To: materials-welding@googlegroups.com
Subject: Re: [MW:22422] G type consumable

The A-number is not assigned. It is determined on the basis of the actual chemical composition of the weld metal.
For certain processes (GMAW, SAW, ....) a chemical analysis of the weld metal is required.

    best regards

    Dr. Georgios Dilintas

    Authorized Nuclear Inspector
    Authorized Inspector Supervisor


    I&F REGIONAL TECHNICAL MANAGER
    BUREAU VERITAS HELLAS

    Tel: +30 210 40 63 113/4
    Fax: +30 210 40 63 118
    Cell: +30 69 44 64 62 04
    (See attached file: Dilintas_George.vcf)

John Henning ---28/11/2014 19:16:59---A -G consumable does not meet any particular ASME/AWS SFA/A-5.x classification chemistry.  This does

From: John Henning <jhenning@deltak.com>
To: "materials-welding@googlegroups.com" <materials-welding@googlegroups.com>
Date: 28/11/2014 19:16
Subject: Re: [MW:22400] G type consumable
Sent by: materials-welding@googlegroups.com




A -G consumable does not meet any particular ASME/AWS SFA/A-5.x classification chemistry.  This does not mean that it will not meet a Section IX A-Number chemistry range.  You would need to evaluate the filler metal manufacturer's specified chemistry range to see if it fits one of the A-number chemistry ranges.  Alternatively, you can specificy that the filler metal must meet a certain range.  While not a G filler metal, I typically specify that ER70S-6 must meet the A-Number 1 chemistry requirements.



From: materials-welding@googlegroups.com <materials-welding@googlegroups.com> on behalf of Pravin Poornachandran <htcispravin@gmail.com>
Sent:
 Friday, November 28, 2014 5:58 AM
To:
 materials-welding@googlegroups.com
Subject:
 [MW:22396] G type consumable 
 
Dear expert,
Is it true that all G type consumable example ER70S-G don't have A number under ASME?
This group only have F number? Is it true?
Kindly advice.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at
http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm

The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to
materials-welding+unsubscribe@googlegroups.com.
For more options, visit
https://groups.google.com/d/optout.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at
http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm

The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to
materials-welding+unsubscribe@googlegroups.com.
For more options, visit
https://groups.google.com/d/optout.

This message contains confidential information. To know more, please click on the following link: http://disclaimer.bureauveritas.com

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...