Wednesday, October 29, 2014

Re: [MW:22192] Rust on Stainless Steel Weld Joints

Dear All,

 

If the rust stains also observed in the pipe itself as well as on the weld joints. What would be the root cause for that.

Dust observed on the pipe. is that may the reason for the rust stains and what the suspected deterioration rate for that.

How to prevent all of these?

 

Thanks.


On Mon, Oct 27, 2014 at 2:20 PM, 'Agustin Jimenez' via Materials & Welding <materials-welding@googlegroups.com> wrote:
Hi
I recomended clean whith citric acid if rust is deep, remove the weld .

Agustin jiménez
Level 2 Ut, rt , pt, vt, mt
CWI


'Prakash Hegde' via Materials & Welding <materials-welding@googlegroups.com> escribió:

>Hi!
>In addition to improper use of Wire brush,Excessive grinding caused the removal of Cr Oxide film and after that Improper Pickling and passivation causes such type of rusted surface
>Regards
>
>Hegde Prakash
>
>
>
>--------------------------------------------
>On Sun, 26/10/14, Vino Varghese <vinopvarghese@gmail.com> wrote:
>
> Subject: Re: [MW:22173] Rust on Stainless Steel Weld Joints
> To: materials-welding@googlegroups.com
> Date: Sunday, 26 October, 2014, 8:27 PM
>
> Hi!!
> Most probably the wire brush/grinding wheel
> (Carbon Steel) would have played the culprit.
> Please check that SS wire brush of good quality
> has been used.
> RegardsVino
>
> On Sat, Oct 25, 2014
> at 10:55 PM, Weaver, mark <Mark.Weaver@honeywell.com>
> wrote:
>
>
>
>
>
> Incorrect filler metal or contaminated brush/grinding
> discs. PMI the weld metal to determine metallurgy. 
>
>
>
> Sent from my iPhone
>
>
> On Oct 25, 2014, at 10:51 AM, "Sahavas v s" <sahavas143r@gmail.com>
> wrote:
>
>
>
>
>
>
> Hi,
>
>
>
> It has been observed on all weld joints were corroded with
> rust, but components dont have any rust. can any one answer
> me the reason why weld joints have only corrosion not on
> base metal?
>
>
>
> Pipe : A312 TP 316 L
>
> Filler wire : ER316L
>
> Weld Type : Butt weld
>
> --
>
> To post to this group, send email to
> materials-welding@googlegroups.com
>
> To unsubscribe from this group, send email to
> materials-welding+unsubscribe@googlegroups.com
>
> For more options, visit this group's bolg at
> http://materials-welding.blogspot.com/
>
> http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
>
>  
>
> The views expressed/exchnaged in this group are members
> personel views and meant for educational purposes only,
> Users must take their own decisions w.r.t. applicable
> code/standard/contract documents.
>
> ---
>
> You received this message because you are subscribed to the
> Google Groups "Materials & Welding" group.
>
> To unsubscribe from this group and stop receiving emails
> from it, send an email to
> materials-welding+unsubscribe@googlegroups.com.
>
> For more options, visit https://groups.google.com/d/optout.
>
>
>
>
>
>
>
>
> --
>
> To post to this group, send email to materials-welding@googlegroups.com
>
> To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
>
> For more options, visit this group's bolg at http://materials-welding.blogspot.com/
>
> http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
>
>  
>
> The views expressed/exchnaged in this group are members
> personel views and meant for educational purposes only,
> Users must take their own decisions w.r.t. applicable
> code/standard/contract documents.
>
> ---
>
> You received this message because you are subscribed to the
> Google Groups "Materials & Welding" group.
>
> To unsubscribe from this group and stop receiving emails
> from it, send an email to materials-welding+unsubscribe@googlegroups.com.
>
> For more options, visit https://groups.google.com/d/optout.
>
>
>
>
>
>
> --
>
> To post to this group, send email to
> materials-welding@googlegroups.com
>
> To unsubscribe from this group, send email to
> materials-welding+unsubscribe@googlegroups.com
>
> For more options, visit this group's bolg at http://materials-welding.blogspot.com/
>
> http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
>
>  
>
> The views expressed/exchnaged in this group are members
> personel views and meant for educational purposes only,
> Users must take their own decisions w.r.t. applicable
> code/standard/contract documents.
>
> ---
>
> You received this message because you are subscribed to the
> Google Groups "Materials & Welding" group.
>
> To unsubscribe from this group and stop receiving emails
> from it, send an email to materials-welding+unsubscribe@googlegroups.com.
>
> For more options, visit https://groups.google.com/d/optout.
>
>
>--
>To post to this group, send email to materials-welding@googlegroups.com
>To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
>For more options, visit this group's bolg at http://materials-welding.blogspot.com/
>http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
>
>The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
>---
>You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
>To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
>For more options, visit https://groups.google.com/d/optout.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm

The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...