Re: [MW:22138] ASME full form of SA - A 387/A 387M - 06a

P91 stands for grade of the material , where P stands for pipe, 91 stands for 9% Cr, 1% Mo and Vanadium . P  no. Of grade P91 material is 15E.

Grade P9 has composition 9% Cr - 1% Mo whose P no. Is 5B.

Regards,
Anup N K E

On 17 Oct 2014 11:18, "Harish Kannepalli" <harishkannepalli@gmail.com> wrote:
American Society of Mechanical Engineers Section A, Developed by ASTM Commitee A01.11 A387/A387M is adopted from ASTM A387/387M where M stands for Metric; as Americans follow inch-pound system; 06 is year of publication, a-is first revision in that year
P91-P is desgination; 9%-Chromium, 1%Molybdenum

2014-10-17 10:40 GMT+04:00 Akhilesh singh <prof.akhileshsingh@gmail.com>:
Plz help me regarding such full-form:

1. ASME full form of SA - A 387/A 387M – 06a ............. what does means of "SA" - "A" 387 ................. "A387M" - "06a"..........................???

                          or
             A 387/A 387M – 06a

2. Grade P91 steel (A 387/A 387M – 06a)
    what does me "P"  & "91"

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.



--
Regards,
Mr. Harish.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...