Hi,
First check with client spec and their requirement, then look in to the pipe category, pressure ratings, pressure class and design criteria for joint efficiency.
In Each of the aspect you have to cross check with the % of RT and should comply to all.
And finally RT is carrying for cross checking the weld quality and not for any of the sake, hence your WPS,WPQ will also influence the % of RT.

Thanks and regards,
Lakshman Kumar.B
9440031459

From: tugrulhan özdemir
Sent: ‎27-‎10-‎2014 16:05
To: materials-welding@googlegroups.com
Subject: [MW:22178] Underground Piping/Pipeline RT %

Dear members


Is there anyone knows a code or standard mentioning the RT percentage for undergorund Piping or pipeline.




Regards



Tugrulhan OZDEMIR
API 653 Ins.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...