Hi dear in my opinion as per asme b31.3 explained  1.5 to 3 mm allowed.

On Wednesday, November 30, 2011 12:51:50 PM UTC+3, md jamil ahmad wrote:
Dear All,
          Any body explain me,1) what is the minimum acceptance criteria for out side weld reinforcement for power piping or process piping
          I think,in general 1.6 to 3mm,is it correct or not.
         2) In inside welding of pipe what is the minimum and maximum reinforcement criteria,please tell me as per ASME Code.


REGARD
JAMIL AHMAD
KSA

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35633] IP Joint

Hello experts, I would like to know what is IP joints in piping(31.3)?  Regards Saurabh -- https://materials-welding.blogspot.com/...