[MW:22148] Re: IQI 1B or IQI 1A?

Please read second last para as set A for film side.
On 19 Oct 2014 20:50, "Shridev Kurup" <shridevk20@gmail.com> wrote:
>
> Dear mohamed,
>
> Asme section V article T-276.2 (a) The thk on which IQI is based is the nominal single wall thickness + applicable estimated weld reinforcement not to exceed the maximum permitted by design code applicable.The actual measurement of the weld reinforcement is not required.
>
> Now in your case thk 5.54 + 1.6 mm(check) = 7.14 mm.If you refer table T-276, correspondence wire type essential wire is 6 source side and film side essential wire is 5.
>
> As per table T- 233.2 Set A & B both having commen wire no 6.For DWDI pipe only source side placement of iqi allowed.
>
> As long as if used Set B IQI and visible wire is 6 th one then required  sensitivity is achieved. Acceptable if source side IQI used.
>
> Both IQI can be used Set A and Set B if required 6th wire source side and set B for film side.
>
> Please check the applicale design code asme 31.3 and Sev Viii for applicable reinforcement for the thickness .
>
> Regards
> Shridev
>
> On 19 Oct 2014 13:33, "weldinguide" <wgadmin@weldinguide.com> wrote:
> >
> > Dear all,
> >
> > Please be informed that our member "mohd" has posted a topic regarding RT IQI. Please have a look at that link
> > IQI 1B or IQI 1A?
> > and kindly let the weldinguide community have your comments.
> >
> > Τhanks in advance for your participation in resolving that issue
> > Best regards
> > The weldinguide Team
> >
> >
> >
> >
> >
> >

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...