Hi,
Its not only WPS matter, welder also need to be qualified with respect to the approved WPS.

Thanks and regards,
Lakshman Kumar.B
9440031459

From: Asif Raza
Sent: ‎22-‎10-‎2014 09:03
To: materials-welding@googlegroups.com
Subject: RE: [MW:22160] WPS for Support

Dear you need to qualify for TIG process as per ASME Sec-IX.

 

John

QC Weld Eng:

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of tugrulhan özdemir
Sent: Tuesday, October 21, 2014 2:47 PM
To: materials-welding@googlegroups.com
Subject: Re: [MW:22158] WPS for Support

 

I think you may check and find suitable sWPS from ASME Sec. IX  and  submit it for approval to your client for only this job.

Regards

Tugrulhan OZDEMIR

QA/QC Welding Eng.


Saygılarımla / Regards

 

Tuğrulhan ÖZDEMİR

API 653 AI, Welding & Materials Eng.

Iraq mobile number: +964 782 311 67 81

 

 

2014-10-20 10:07 GMT+03:00 Richard robes <mech.processes@gmail.com>:

Dear ALL,

 

Please comment on the issue, Pipe to Shoe support fillet welding - Have WPS for SMAW process, can a welder do pipe to shoe support fillet welding in GTAW process.

Please note that for this specific project we don't have a wps qualified for GTAW process, only qualified wps for SMAW process.

 

Awaiting replies !

 

Regards

Richard

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...