[MW:22183] Re: Bend angle

Hello,

Minimum bend radius depends of your design code, pipe's diameter, allowable stress, thickness; when inspecting look for buckling, cracks, and else. In the field the angle is function of the profile.

http://books.google.com.co/books?id=rq69qn9WpQAC&pg=PA52&lpg=PA52&dq=cold+bend+radius+pipe&source=bl&ots=KV2jASYjEQ&sig=oTqrX_bLBRZ3xTjnULO9F4ytmZY&hl=en&sa=X&ei=gghPVKiNJ4magwS0lIHYDQ&redir_esc=y#v=onepage&q=cold%20bend%20radius%20pipe&f=false


Sergio Antonio Muñoz Pinzón
IWE-IIW
http://Weld-ING.blogspot.com

El lunes, 27 de octubre de 2014 12:16:56 UTC-5, balaji escribió:

Dear all,
I would like to know for field cold bending what are the inspection points need to check.also in the drawing bending angle only mentioned how to calculate get radious and ensuring that            please advice me.

Thanks in advance.

Regards,
Balaji

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...