Dear Laxman,
i m using.this pipe with a pump. Pressure is about 80 bar. Yes its above ground. The water has some silt content. The silt size is about 300 mesh.
On Tuesday, October 28, 2014, Lakshman <lakshmankumar4@gmail.com> wrote:
> Hi,
> Please let the issue elobarated further to anyalyse in detail like as....
> Operating Pressure,and velocities
> Under ground or above ground
> Sweet water or sea water
> Pipe joining facilitation
> Pipe Dia to check the fieasability for any coating etc
>
> Thanks and regards,
> Lakshman Kumar.B
> 9440031459
> ________________________________
> From: Kadir godil
> Sent: 28-10-2014 16:44
> To: materials-welding@googlegroups.com
> Subject: [MW:22185] material/grade of pipe for water with minor silt
>
> dear experts,
> i require your help in selecting a piping grade for water containing minor silt. i am afraid of erosion inside the pipe. which grade should i select?
> if you can mention ASTM grade it will be of great help.
> thank you.
> sincerely,
> kadir
>
> --
> To post to this group, send email to materials-welding@googlegroups.com
> To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
> For more options, visit this group's bolg at http://materials-welding.blogspot.com/
> http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
>
> The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
> ---
> You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
> To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
> For more options, visit https://groups.google.com/d/optout.
>
> --
> To post to this group, send email to materials-welding@googlegroups.com
> To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
> For more options, visit this group's bolg at http://materials-welding.blogspot.com/
> http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
>
> The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
> ---
> You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
> To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
> For more options, visit https://groups.google.com/d/optout.
> --
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.
i m using.this pipe with a pump. Pressure is about 80 bar. Yes its above ground. The water has some silt content. The silt size is about 300 mesh.
On Tuesday, October 28, 2014, Lakshman <lakshmankumar4@gmail.com> wrote:
> Hi,
> Please let the issue elobarated further to anyalyse in detail like as....
> Operating Pressure,and velocities
> Under ground or above ground
> Sweet water or sea water
> Pipe joining facilitation
> Pipe Dia to check the fieasability for any coating etc
>
> Thanks and regards,
> Lakshman Kumar.B
> 9440031459
> ________________________________
> From: Kadir godil
> Sent: 28-10-2014 16:44
> To: materials-welding@googlegroups.com
> Subject: [MW:22185] material/grade of pipe for water with minor silt
>
> dear experts,
> i require your help in selecting a piping grade for water containing minor silt. i am afraid of erosion inside the pipe. which grade should i select?
> if you can mention ASTM grade it will be of great help.
> thank you.
> sincerely,
> kadir
>
> --
> To post to this group, send email to materials-welding@googlegroups.com
> To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
> For more options, visit this group's bolg at http://materials-welding.blogspot.com/
> http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
>
> The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
> ---
> You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
> To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
> For more options, visit https://groups.google.com/d/optout.
>
> --
> To post to this group, send email to materials-welding@googlegroups.com
> To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
> For more options, visit this group's bolg at http://materials-welding.blogspot.com/
> http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
>
> The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
> ---
> You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
> To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
> For more options, visit https://groups.google.com/d/optout.
> --
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.
Comments