Please let the issue elobarated further to anyalyse in detail like as....
Operating Pressure,and velocities
Under ground or above ground
Sweet water or sea water
Pipe joining facilitation
Pipe Dia to check the fieasability for any coating  etc

Thanks and regards,
Lakshman Kumar.B
9440031459

From: Kadir godil
Sent: ‎28-‎10-‎2014 16:44
To: materials-welding@googlegroups.com
Subject: [MW:22185] material/grade of pipe for water with minor silt

dear experts,

i require your help in selecting a piping grade for water containing minor silt. i am afraid of erosion inside the pipe. which grade should i select? 

if you can mention ASTM grade it will be of great help.

thank you.

sincerely,
kadir

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...