Re: [MW:17233] WPS with PWHT below the lower transformation temperature

Dear Mohd.,

As per ASME B-31.3 Table 331.1.1 you have to do PWHT within the specified range of 593 deg C to 649 deg C (for P-No-1) you can not do or write beyond that limits.



On Sat, Mar 23, 2013 at 10:20 AM, mohd <mohd52100@gmail.com> wrote:

Dear all,

WPS details as per ASME IX  Design Code :B31.3

1) GTAW + SMAW (3mm+ 24mm)
2) Material API 5L x52 Thk : 26.97
3) PWHT 600 +/-20  Time : 1Hr  20min
4) No impact.
 
Can I Re Write WPS with Temperature  670+/-20 as per As per QW-407.1 a (2) ? ( up to below Lower transformation no need re qualification )

Need expert Opinion.

QW-407 Postweld Heat Treatment
QW-407.1 A separate procedure qualification is
required for each of the following:
(a) For P-Numbers 1 through 6 and 9 through 15F materials,
the following postweld heat treatment conditions
apply:
(1) no PWHT
(2) PWHT below the lower transformation temperature )



Regards,
mohd.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
 
 



--
Thanks & Regards
Biplab Pal
Welding Inspector
E-mail:   biplab.mech@gmail.com
 
Information in this email and any attachments is confidential and intended solely for the use of the individual(s) to whom it is addressed or otherwise directed. Please note that any views or opinions presented in this email are solely those of the author and do not necessarily represent those of the Company. Finally, the recipient should check this email and any attachments for the presence of viruses. Myself accepts no liability for any damage caused by any virus transmitted by this email.
 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
 
 

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...