[MW:17240] Re: ASME SA 333 Gr. 6 Chemical composition

Dear All Experts,

Please provide your feedback for below query with some technical justification or code reference.

 

Thanks & Regards,

Mohd. Azam


On Tue, Mar 19, 2013 at 5:09 PM, Azam Mohd <azam1976@gmail.com> wrote:

Dear Experts,

ASME Section II Part A Edition 2010

ASME SA 333/SA 333M

 

The Pipe material is ASME SA 333 Gr.6, as per clause 5.2 and Table-1 the allowable chemical element is C, Mn, P, S, Si only

As per material MTC chemical element is C (0.17%), Mn (093%), P (0.010), S (0.0010), Si (0.24), Cu(0.050%), Cr (0.12%), Ni (0.060%), Mo(0.020%), V(less than 0.004%).

 

Our query is weather above chemical element (MTC) can be accepted for ASME SA333 Gr.6.

 

Looking forward to see the comment from Mr.Pradip Goswami on above matter.

 

Thanks & Regards,

Mohd. Azam

Doha-Qatar



On Wed, Mar 13, 2013 at 3:35 PM, Azam Mohd <azam1976@gmail.com> wrote:

Dear Experts,

The below material chemical composition for ASME SA 333 Gr. 6 as per MTC

 

 

But as per ASME SA 333 Gr.6, Allowable chemical element C, Mn, P, S, Si only. Please refer ASME Section II Part A Edition 2010 clause 5.2.

 

Need your comment weather this chemical composition can be accepted. Please provide the technical clarification or code reference.

 

Thanks & Regards,

Mohd. Azam




--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
 
 

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...