you should give the standard type written on the rail parts and search about that type material to know the electrode required.
Eng\ Ansary
email:ansary_77@hotmail.com
Mobile :01283667723-01114206108
From: A.osman81@yahoo.ca
To: materials-welding@googlegroups.com
Subject: [MW:17213] Welding Train Rail to CS base Plate
Date: Mon, 25 Mar 2013 18:07:19 +0300
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
Eng\ Ansary
email:ansary_77@hotmail.com
Mobile :01283667723-01114206108
From: A.osman81@yahoo.ca
To: materials-welding@googlegroups.com
Subject: [MW:17213] Welding Train Rail to CS base Plate
Date: Mon, 25 Mar 2013 18:07:19 +0300
Dears
I face a problem in my site … I have a rail do not know its material … we need to weld this rail to CS base plate (fillet weld) .. I told them to use E9018-D1 but it was not available they use 7018-1 but joints is cracked … please confirm me the electrode to use
** the rail is from Turkish railways rails
Ahmed
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
Comments