Hi
 
Please refer ASTM A 262.
 
Regards
 
Prem Nautiyal
Cell: 9769316004

From: Venkatesh <vpv_333@yahoo.com>
To: materials-welding@googlegroups.com
Sent: Monday, March 25, 2013 11:48 AM
Subject: [MW:17211] IGC Practice A and E
Dear Expert,
 
What is the difference between IGC practice 'A' and 'E'?
 
Which is recommended for Austenitic stainless steels?
Thanks & Regards

P.Venkatesh
-- To post to this group, send email to materials-welding@googlegroups.comTo unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.comFor more options, visit this group's bolg at http://materials-welding.blogspot.com/http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.--- You received this message because you are subscribed to the Google Groups "Materials & Welding" group.To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.For more options, visit https://groups.google.com/groups/opt_out.  

No comments:

[MW:35633] IP Joint

Hello experts, I would like to know what is IP joints in piping(31.3)?  Regards Saurabh -- https://materials-welding.blogspot.com/...