Monday, March 25, 2013

RE: [MW:17211] regarding welder performance qualification

If u want welder qualification u must follow section XI and if u want
electrode qualification u have to follow sec II C.

-----Original Message-----
From: materials-welding@googlegroups.com
[mailto:materials-welding@googlegroups.com] On Behalf Of kannayeram
gnanapandithan
Sent: 25 March 2013 11:23
To: materials-welding@googlegroups.com
Subject: Re: [MW:17208] regarding welder performance qualification

Pl qualify one procedure according to ASME sec 9 Pandithan Welding
Consultant

On 3/25/13, chandan choudhary <choudharyck7630@gmail.com> wrote:
> dear experts,
>
> i am working in consumable industry where we followed ASME SEC.II C
> only.For the performance of electrode & other mechanical testing we
> have 7 welders.now a days we are facing a problem about welder
> performance qualification.As we know that for welder qualilication we
> followed ASME sec.ix and for this we need one approved WPS according
> to sec.ix .my query is that can i use WPS made according to sec.iic
> instead of sec.ix. if yes,then please let me know where it is mentioned?
>
>
> Thanks & regards,
>
> chandan kr. choudhary
> ADOR WELDING LTD
> 7567954462
>
> --
> To post to this group, send email to
> materials-welding@googlegroups.com
> To unsubscribe from this group, send email to
> materials-welding+unsubscribe@googlegroups.com
> For more options, visit this group's bolg at
> http://materials-welding.blogspot.com/
> http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=12278
> 7&trk=anet_ug_hm
>
> The views expressed/exchnaged in this group are members personel views
> and meant for educational purposes only, Users must take their own
> decisions w.r.t. applicable code/standard/contract documents.
> ---
> You received this message because you are subscribed to the Google
> Groups "Materials & Welding" group.
> To unsubscribe from this group and stop receiving emails from it, send
> an email to materials-welding+unsubscribe@googlegroups.com.
> For more options, visit https://groups.google.com/groups/opt_out.
>
>
>

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to
materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at
http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=
anet_ug_hm

The views expressed/exchnaged in this group are members personel views and
meant for educational purposes only, Users must take their own decisions
w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups
"Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an
email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm

The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...