Dear sir,
Actually asme 9 is based for welding procedural while section IIC for
material properties.
So please you can move with ASME 9.
REGARDS
DINESH
-----Original Message-----
From: materials-welding@googlegroups.com
[mailto:materials-welding@googlegroups.com] On Behalf Of kannayeram
gnanapandithan
Sent: Monday, March 25, 2013 9:53 AM
To: materials-welding@googlegroups.com
Subject: Re: [MW:17208] regarding welder performance qualification
Pl qualify one procedure according to ASME sec 9
Pandithan
Welding Consultant
On 3/25/13, chandan choudhary <choudharyck7630@gmail.com> wrote:
> dear experts,
>
> i am working in consumable industry where we followed ASME SEC.II C
> only.For the performance of electrode & other mechanical testing we have 7
> welders.now a days we are facing a problem about welder performance
> qualification.As we know that for welder qualilication we followed ASME
> sec.ix and for this we need one approved WPS according to sec.ix .my query
> is that can i use WPS made according to sec.iic instead of sec.ix. if
> yes,then please let me know where it is mentioned?
>
>
> Thanks & regards,
>
> chandan kr. choudhary
> ADOR WELDING LTD
> 7567954462
>
> --
> To post to this group, send email to materials-welding@googlegroups.com
> To unsubscribe from this group, send email to
> materials-welding+unsubscribe@googlegroups.com
> For more options, visit this group's bolg at
> http://materials-welding.blogspot.com/
>
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=
anet_ug_hm
>
> The views expressed/exchnaged in this group are members personel views and
> meant for educational purposes only, Users must take their own decisions
> w.r.t. applicable code/standard/contract documents.
> ---
> You received this message because you are subscribed to the Google Groups
> "Materials & Welding" group.
> To unsubscribe from this group and stop receiving emails from it, send an
> email to materials-welding+unsubscribe@googlegroups.com.
> For more options, visit https://groups.google.com/groups/opt_out.
>
>
>
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to
materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at
http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=
anet_ug_hm
The views expressed/exchnaged in this group are members personel views and
meant for educational purposes only, Users must take their own decisions
w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups
"Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an
email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
Subscribe to:
Post Comments (Atom)
[MW:35668] Selection of Filler/Electrode.
Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...
-
Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? ...
-
Definition of buttering from ASME Section IX, QW/QB-492 Definitions: Buttering: the addition of material, by welding, on one or bot...
-
Section I. PRINT READING 3-1. GENERAL a. Drawings . Drawing or sketching is a universal language used to convey all necessary information to...
No comments:
Post a Comment