I think the max thickness qualified is the coupon thickness for your job in accordance with api 1104 sec12.
If your welding process is manual, then you have to consider sec 5 of api 1104



On Wednesday, March 20, 2013, mohd <mohd52100@gmail.com> wrote:
> Dear ali,
> Means U have establish 4.8mm to 19mm any changes from beyond that req requalification. Please note that as per API Diameter is non essential( u can switches from one group to another group dia within thickeness range example OD less than 2.375 in WPS   TO NEW WPS OD 2.375 in.through 12.750 in with same thickenss range.)
> 12.5.2.4 Wall Thickness
> A change in wall thickness beyond the range established in
> the procedure specification constitutes an essential variable
> 5.4.2.5 Wall Thickness
> A change from one wall thickness group to another constitutes
> an essential variable.
> Regards,
> Mohd
> On Monday, March 18, 2013 7:46:36 AM UTC+3, alisamdani wrote:
>>
>> Dear All,
>>
>> Please guide me about interpretation of clause 12.5.2.4 of API 1104
>> regarding wall thickness of Automatic welding process which states "a
>> change in wall thickness beyond the range established in the procedure
>> specification constitutes an essential variable"
>> In my PQR sample thickness is 12.7 mm process is GMAW (STT)/FCAW.  If
>> I specify thickness range from 4.8 to 19.1 mm (group "b" of API) will
>> it be OK?
>> Please give your interpretation/thoughts of above clause what would be
>> my qualified thickness range with using above PQR thickness.
>>
>> Thanks in advance
>> Ali Samdani
>
> --
> To post to this group, send email to materials-welding@googlegroups.com
> To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
> For more options, visit this group's bolg at http://materials-welding.blogspot.com/
> http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
>  
> The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
> ---
> You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
> To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
> For more options, visit https://groups.google.com/groups/opt_out.
>  
>  
>

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
 
 

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...