[MW:17165] Re: Welding of Weldox 700 plate with backing

Mr Tugrul,
 
i think you may try ER100 SG for root and ER110 SG for upper layer.

18 Mart 2013 Pazartesi 14:22:25 UTC+2 tarihinde tugrulhan özdemir yazdı:
Dear  welding peole
 
 
We had Weldox 700 plate with 6 mm thickness, using GMAW method with backing.
 
First we made:    2  passes  with ER110SG   (1.2 dia wire) with backing : failed ( root bending)
Second         :     3 passes  with ER110SG (1.2 dia wire) with backing  and pre heating(25 C) : failed (root bending)
 
We will try for the 3rd time.  I am planing to use :
 
ER100SG (1 mm  dia wire)  with backing ------------ root run
ER110SG (1mm dia wire) with backing    ------------ all other  
we will apply preheat also (around 25 C)
 
 
Is there anyone has experience about 6mm weldox 700 with backing. Do you have any PQR and WPS ?
 
 
Regards
 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
 
 

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...