Saturday, March 23, 2013

Re: [MW:17203] API 1104 Wall thickness qualification for Auto-welding

GMAW(STT) is semi-auto while FCAW is automatic. root is with GMAW(STT)
and fill/cap is with FCAW.

On Sat, Mar 23, 2013 at 9:42 AM, Samun Bhatia <samunbhatia@gmail.com> wrote:
> Dear all,
> 1st u have to check that both process r automatic or semiautomatic
>
> On Mar 18, 2013 11:14 AM, "M.A.Samdani" <m.a.samdani7@gmail.com> wrote:
>>
>> Dear All,
>>
>> Please guide me about interpretation of clause 12.5.2.4 of API 1104
>> regarding wall thickness of Automatic welding process which states "a
>> change in wall thickness beyond the range established in the procedure
>> specification constitutes an essential variable"
>> In my PQR sample thickness is 12.7 mm process is GMAW (STT)/FCAW. If
>> I specify thickness range from 4.8 to 19.1 mm (group "b" of API) will
>> it be OK?
>> Please give your interpretation/thoughts of above clause what would be
>> my qualified thickness range with using above PQR thickness.
>>
>> Thanks in advance
>> Ali Samdani
>>
>> --
>> To post to this group, send email to materials-welding@googlegroups.com
>> To unsubscribe from this group, send email to
>> materials-welding+unsubscribe@googlegroups.com
>> For more options, visit this group's bolg at
>> http://materials-welding.blogspot.com/
>>
>> http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
>>
>> The views expressed/exchnaged in this group are members personel views and
>> meant for educational purposes only, Users must take their own decisions
>> w.r.t. applicable code/standard/contract documents.
>> ---
>> You received this message because you are subscribed to the Google Groups
>> "Materials & Welding" group.
>> To unsubscribe from this group and stop receiving emails from it, send an
>> email to materials-welding+unsubscribe@googlegroups.com.
>> For more options, visit https://groups.google.com/groups/opt_out.
>>
>>
> --
> To post to this group, send email to materials-welding@googlegroups.com
> To unsubscribe from this group, send email to
> materials-welding+unsubscribe@googlegroups.com
> For more options, visit this group's bolg at
> http://materials-welding.blogspot.com/
> http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
>
> The views expressed/exchnaged in this group are members personel views and
> meant for educational purposes only, Users must take their own decisions
> w.r.t. applicable code/standard/contract documents.
> ---
> You received this message because you are subscribed to the Google Groups
> "Materials & Welding" group.
> To unsubscribe from this group and stop receiving emails from it, send an
> email to materials-welding+unsubscribe@googlegroups.com.
> For more options, visit https://groups.google.com/groups/opt_out.
>
>

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm

The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...