Dear sir,

 

Please read asme 9 & along with aws d1.1.First read aws d 1.1 so it will be easy to understand an some sort of information.

 

Regards

Dinesh

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of chandrakant mohikar
Sent: Friday, March 22, 2013 10:32 AM
To: materials-welding@googlegroups.com
Subject: Re: [MW:17193] How to make WPS & PQR

 

You need to specify co. requirements for preparation.

 

you may refer

 

QW 100, 200 articles in ASME sec. IX

 

Chandrakant Mohikar (PMC)

(ex. Project-QA, PDO/ VELOSI Oman)

 

On Thu, Mar 21, 2013 at 11:08 PM, BRIJESH KUMAR SINGH <brijeshkumarsingh1986@gmail.com> wrote:

Dear seniors
I regularly fallow your all E-mails and query. Can any bady tel me how to prepare WPS & PQR.
I will really appropriate you if anyone help me for the above.

Thanks in advance

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
 
 

 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
 
 

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...