Tuesday, February 19, 2013

RE: [MW:16808] SWPS

Dear Riaz,

 

SWPS= Standard Welding procedure specifications

For more details, you may please refer ASME Section IX (Article V)

AWS D1.1 -part 3 describes prequalified WPSs, which is same as SWPS.

 

 

 

 

Thanks & Regards,

      TEAM QA/QC- SHOAIBA II CCPP

       S.Binoy, Welding Engineer  

     DAELIM Saudi Arabia Co. Ltd.

     Email- binoy.spp@daelim.co.kr

       Mob: 0592633853 / 0508308633

                   

                       Let Us Believe in TEAM Work (Together   E veryone   Achieves  More)”

 

 

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Ri@z
Sent: Tuesday, February 19, 2013 8:33 AM
To: materials-welding@googlegroups.com
Subject: [MW:16801] SWPS

 

hellow masters,

 

What is this SWPS means..??

 

Is it possible to purchase SWPS from ASME??

 

With regards

 

Riaz

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
 
 

No comments:

[MW:35748] Re: PQR- Chemical testing requirements

As answered by everyone, chemical is not required. Notwithstanding, please note that A-No. which denotes weld metal chemical composition is ...