Sunday, January 1, 2012

Re: [MW:13377] Room Temp/High temp Properties & allowable stresses in P92 pipes

I will check the 2011 adenda.
Happy new year
Best regards
Dr Georgios Dilintas
Authorized Nuclear Inspector
Authorized Inspector Supervisor
HBS Regional Technical Manager


  From: "pgoswami" [pgoswami@quickclic.net]
  Sent: 31/12/2011 00:22 EST
  To: <materials-welding@googlegroups.com>
  Cc: George Dilintas; <vbarora@gamail.com>
  Subject: RE: [MW:13372] Room Temp/High temp Properties & allowable stresses in P92 pipes


Dr Dilintas and Mr. Arora,
 
I am referring to Sec-II, Pt-D, 2010 edition( effective date 01 July). This material is included in Sec-II Pt-A, e.g SA 213, but till 01 July, P-92 material was not included in the stress tables , in Sec-II, Pt-D.
 
SAME code case  2179-7 (approval date Jan, 2009) provides details on the stress value of this steel, including compositions and heat treatment.
 
I'm not sure about the updates, as I don't have them handy, I absence of code updates one could follow the above code case.
 
Thanks.
 
 
Pradip Goswami,P.Eng.IWE
Welding & Metallurgical Specialist & Consultant
Ontario,Canada.
Email-pgoswami@sympatico.ca,
 


From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of george.dilintas@gr.bureauveritas.com
Sent: Friday, December 30, 2011 5:41 AM
To: materials-welding
Subject: Re: [MW:13366] Room Temp/High temp Properties & allowable stresses in P92 pipes

Check in ASME section II-A and II-D
Best regards
Dr Georgios Dilintas
Authorized Nuclear Inspector
Authorized Inspector Supervisor
HBS Regional Technical Manager


  From: Ved Bhushan Arora [vbarora48@gmail.com]
  Sent: 30/12/2011 09:52 ZE5B
  To: materials-welding@googlegroups.com
  Subject: [MW:13365] Room Temp/High temp Properties & allowable stresses in P92 pipes


Dear All
 
I need the P92 pipe material properties , physical , mechanical, high temp & allowable stresses etc.
 
Thanks
 
Ved Bhushan Arora

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35763] Hardness range for CS+ Alloy0625 clad welding

Dear experts. I am currently in the process of qualifying a PQR for API 5L X65 + A350 LF6. Both material consists of a base metal with alloy...