Monday, January 23, 2012

[MW:13545] Maraing steel with eutectoid steel


Hi all,

We are trying to weld 300 grade maraging steel with eutecoid steel.
I tried to find some welding literature on this two steel, but no one has done it.

I like to know,
##   What will be the welding parameters to have a good weld deposit.  ##
##  What preheat temperature ##
## What inter-run temperature have to be maintained ##
## If you send some link related to it, then it help me out. ##


welding dimension : 70mm in length , 20mm wedth, and 15 mm depth.

Chemical Composition

Maraging steel Consumables 2.5 dia
 

Element

C

Mn

Si

P

S

Ni

Co

Mo

Ti

Al

Cr

Wt%

0.03

0.10

0.10

0.010

0.010

18

9

5

0.6

0.10

0.50

Cu

0.50

 


Eutecoid steel :

Element

C

P

Mn

Si

S

Ni

Cr

Mo

Cu

Al

Sn

Wt%

0.64

0.031

0.75

0.15

0.027

0.024

0.062

<0.002

0.041

0.003

0.003



Thank you,

C . R . RATHOD

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...