Thursday, January 26, 2012

Re: [MW:13574] MODE OF METAL TRANSFER IN FCAW PROCESS

Dear Manoj,

Refer last two pages for the Metal transfer modes from the attached Document

Regards,
Vijay

On Tue, Jan 24, 2012 at 12:30 PM, manoj john <manojacgnr@gmail.com> wrote:
Dear All,

I would like to know about mode of  metal transfer in FCAW welding process.  Please share some information regrading short circuting, globular transfer, spray transfer .

Thanks in advance.

Manoj

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

1 comment:

sheikdawood said...

Dear Sir,
Please find out the pipe defect is Root Concavity or Incomplete root fusion please clear for me.

Re: [MW:35686] HDPE WPS