Thursday, January 19, 2012

[MW:13509] Re : WPS for Orbital Welding for Tubes Weld

Dear All,

 

If anybody had sample WPS for Welding Tubes with applied Orbital Welding please share with me..

I need as references to create WPS

 

Regards

Rizal



__________ Information from ESET NOD32 Antivirus, version of virus signature database 6807 (20120118) __________

The message was checked by ESET NOD32 Antivirus.

http://www.eset.com

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...