Skip to main content

Re: [MW:13588] RE: 13556] Welding API 5L X70 By ER 80S-Ni1 + FOX EV 60

Dear Mohamed:

If it is pipeline, go with GMAW or FCAW but if it is a piping spool you'd better use GTAW for root & hot pass and filling & cap with SMAW or FCAW.

Whatever filler metal you use (should be Ni-alloyed), do not exceed the base metal strength by more than 10 ksi since it won't do any good except more cost and care during welding. Check the vendor catalogue for instructions.
  
Ramin  Kondori
   QC/Welding Engineer 
         IWE AT 0070
  


On Thu, Jan 26, 2012 at 7:50 AM, Fitria Rahman <t.chintaqa@gmail.com> wrote:
in most situations, you will receive numerous suggestions with several
electrodes falls under E80XX. If you are not going with PWHT, i would
rather suggest you to go with E81T1.

To me, TIG process is not suitable for large diameter - 30".

Rgds

2012/1/25, Lakshman Kumar.B <lakshmankumar4@gmail.com>:
> DEAR,
>
>
>
> Is GTAW is required?
>
> We used SMAW or GMAW for the root and remaining for with FCAW or GMAW which
> is more economical and good work progress.
>
>
>
> Thanks and Regards................?
>
>
> cid:image001.jpg@01CC3048.5836D9B0
>
> Lakshman Kumar.B|Manager |Lanco Infratech Limited
>
> Plot No 1255 | Sanjeevani chowk | Mahanadi vihar | Cuttack 753004
>
> Phone : + 91 671 2445033 | Mobile : +91 9937286851 |www.lancogroup.com
>
> Go Green|The future will thank you
>
>
>
>
>
> From: materials-welding@googlegroups.com
> [mailto:materials-welding@googlegroups.com] On Behalf Of Mohamed Elsayed (
> BTG)
> Sent: Tuesday, January 24, 2012 9:42 AM
> To: materials-welding@googlegroups.com
> Subject: [MW:13556] Welding API 5L X70 By ER 80S-Ni1 + FOX EV 60
>
>
>
> Dear,
>
>
>
> We have material  API 5L X70 , 30" O.D ; Thk. 13.33mm , we are planning to
> do PQR using ER 80S-Ni1(mod) 2.4mm for GTAW and E8018-C3H4R - Bohler welding
> consumable. Is it correct?
>
>
>
> Please advice.
>
>
>
>
>
> Thanks
>
> Mohamed
>
>
>
> --
> To post to this group, send email to materials-welding@googlegroups.com
> To unsubscribe from this group, send email to
> materials-welding+unsubscribe@googlegroups.com
> For more options, visit this group's bolg at
> http://materials-welding.blogspot.com/
> The views expressed/exchnaged in this group are members personel views and
> meant for educational purposes only, Users must take their own decisions
> w.r.t. applicable code/standard/contract documents.
>
> --
> To post to this group, send email to materials-welding@googlegroups.com
> To unsubscribe from this group, send email to
> materials-welding+unsubscribe@googlegroups.com
> For more options, visit this group's bolg at
> http://materials-welding.blogspot.com/
> The views expressed/exchnaged in this group are members personel views and
> meant for educational purposes only, Users must take their own decisions
> w.r.t. applicable code/standard/contract documents.
>

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...

Re: [MW:10788] ON PLOT PIPING & OFF PLOT PIPING

Piping systems involved for the flow lines and gathering lines from the well head isolation valve to the production facility or processing plant isolation valve are determined as OFF PLOT. ON PLOT defines piping system in the processing plant and production platform. ANSI/ASME B31.4 applies for off plot piping system. B31.4 allows the use of either API 1104 or ASME section IX (as appropriate). However, occasionally, a very small system such as piping within 500 feet of a processing plant (some client also said 400 feet) may be declared B31.3 rather than B31.4. When B31.3 is invoked, only ASME Section IX is used. before you decide which code to use for welding procedure and/or welder qualification for pipe welding, you have to know the design and construction code applicable to the system. Please read far enough into scope and diagram illustrating the application of either B31.3 and B31.4 hope this helps rgds 2011/4/21 pradip kumar sil < pradipsil@gmail.com > Dear all, ...