Friday, January 20, 2012

[MW:13527] RE: 13526] Preheat & Interpass temperature - Reg

Typically preheat recommendations will come from the construction Code
(for example Section I - PW38, Section VIII - Appendix R, or UCS-56
notes). High restraint, or other factors, may result in using a higher
preheat than recommended/specified in the code. General rule of thumb
for interpass; 600F max. for carbon and alloy steels {Q&T or specialty
steels - consult material supplier}, 350F max for stainless, and 300F
max for duplex stainless and nickel based.

John A. Henning
Welding & Materials

-----Original Message-----
From: materials-welding@googlegroups.com
[mailto:materials-welding@googlegroups.com] On Behalf Of Ramesh
Deenathayalan
Sent: Friday, January 20, 2012 1:40 AM
To: materials-welding@googlegroups.com
Subject: [MW:13526] Preheat & Interpass temperature - Reg

Dear friends,

While writing the WPS based on ASME SEC IX, how can we determine the
minimum preheat temperature and maximum interpass temperature?? Kindly
advice.

Ramesh D

Sent from my Nokia phone

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to
materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at
http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views
and meant for educational purposes only, Users must take their own
decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...