Please use ER/E NiCrMo4 welding consumables for GTAW & SMAW processes for welding Hastealloy
and
ER/E NiCrMo3 welding consumables for Hastealloy to SS316L
Thanks & Regards
J.Gerald Jayakumar
0091-9344954677
From: Vivek Pandey <vivek.pande06@gmail.com>
To: materials-welding@googlegroups.com
Cc: pgoswami@sympatico.ca; karthik6684@yahoo.com
Sent: Wednesday, January 18, 2012 11:02 AM
Subject: [MW:13499] Regarding welding consumable for Material hastelloy C276
Dear All
With reference to above subject,kindly suggest me which Consumable is
suitable for welding of hastelloy C276 material( UNS NO: N10276 ).
actually I want to do qualify in two different procedure.
preocedure are as follows
Material: UNS NO:N10276+UNS NO: N10276 PROCESS GTAW+ SMAW
Material: UNS NO:N10276 +SA182 GR 316L PROCESS GTAW+ SMAW
KINDLY CONFORM TO ME AS SOON AS POSSIBLE
Regards
vivek pndey
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
0091-9344954677
From: Vivek Pandey <vivek.pande06@gmail.com>
To: materials-welding@googlegroups.com
Cc: pgoswami@sympatico.ca; karthik6684@yahoo.com
Sent: Wednesday, January 18, 2012 11:02 AM
Subject: [MW:13499] Regarding welding consumable for Material hastelloy C276
Dear All
With reference to above subject,kindly suggest me which Consumable is
suitable for welding of hastelloy C276 material( UNS NO: N10276 ).
actually I want to do qualify in two different procedure.
preocedure are as follows
Material: UNS NO:N10276+UNS NO: N10276 PROCESS GTAW+ SMAW
Material: UNS NO:N10276 +SA182 GR 316L PROCESS GTAW+ SMAW
KINDLY CONFORM TO ME AS SOON AS POSSIBLE
Regards
vivek pndey
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
Comments