Saturday, January 28, 2012

Re: [MW:13578] Ultrasonic Testing & Intergranular Corrosion Testing; G28 Method A for CRO Welding on Carbon Steel with Inconel 625

Inter-granular test required for 625 material. UT is not require.If client spec specify that ut test require , if u have to do Utb test.\


On Sat, Jan 28, 2012 at 10:28 AM, Ghafor Mohamad <ghaformohamad@gmail.com> wrote:
Dear Experts

I am qualified a PQR for CRO Welding using Inconel 625 on Carbon Steel plate. As per ASME IX, mandatory test is:
  1. Dye Penetration Test
  2. Transverse Side Bend Test
  3. Chemical Analysis
  4. Hardness (location may refer to ISO 15056 Fig 6 for NACE req.)
  5. Macro Etch photo

What I am confusing is that Intergranular Corrosion (G28 Method A) and Ultrasonic Test is applicable to conduct or not? 

Thanks

BR; Abdul Ghafor Mohamad


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...