RE: [bulk] [MW:13516] Need to some ASME standard codes reference for Pup Pieces

Hi.
A good practice is 1.5 x diameter or specdification, in AWS D1.1 show distance betwen welds.



Atentamente

Agustin Jimenez

Gerencia de Operaciones

Representaciones y Servicio AGUMAR C.A.

Movil: 0416-7801321 - 04248894456

Twitter: @festejosagumark

Mercadolibre: Festejos Agumarca


 


--- El jue, 1/19/12, Mohamed Elsayed ( BTG) <MElsayed@ccc.ae> escribió:

De: Mohamed Elsayed ( BTG) <MElsayed@ccc.ae>
Asunto: RE: [bulk] [MW:13513] Need to some ASME standard codes reference for Pup Pieces
A: materials-welding@googlegroups.com
Fecha: jueves, 19 de enero de 2012, 05:32 am

Hi,

 

You cannot find in ASME Codes , But that is as per the project specs. Which mentioned The min. distance between the 2 girth welded joints .

Thanks

Mohamed elsayed

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of mpk mpk
Sent: 19 January 2012 07:33
To: materials-welding
Subject: [bulk] [MW:13507] Need to some ASME standard codes reference for Pup Pieces
Importance: Low

 

Dear Experts,

Can any body Give the Minimum length of the Onshore and offshore pup piece fabrication and welding ?

Need to some ASME standard codes reference..

thank you,

MPK

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35633] IP Joint

Hello experts, I would like to know what is IP joints in piping(31.3)?  Regards Saurabh -- https://materials-welding.blogspot.com/...