Tuesday, January 17, 2012

[MW:13498] compatible forging material for SA 527 grade E plate

To the experts,

I am designing steam drum using SA 517 grade E plate material in ASME Sec, VIII, Div. II. For this please suggest me a compatible forging material for designing of nozzles.  

--
Thanks & regards,

Hemant B. Chintamani
Sr. Design Engineer,
ISGEC Heavy Ind. Ltd.,
India.


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...