Tuesday, January 24, 2012

Re: [MW:13554] REGARDING PWHT of STORAGE TANK CLEAN OUT DOOR.

Applicable Code is  ASME SEC IX.
Impact test not required.

On Mon, Jan 23, 2012 at 12:49 PM, james gerald <gerry_tup@yahoo.com> wrote:
Please give the detail of the applicable code and whether Impact test is required based on MDMT
 
Thanks & Regards J.Gerald Jayakumar 0091-9344954677

Sent: Saturday, January 21, 2012 7:55 PM

Subject: [MW:13536] REGARDING PWHT of STORAGE TANK CLEAN OUT DOOR.

Dear All,

I intended to use the following  WPS  for  storage tank clean out door welding :

Test coupon thickness  -   40 mm.
Material                       -   SA 516 Gr 70
Welding process          -   SMAW.
Electrode                    -    E 7018-1
PWHT  Temperature     -   620 - 650 degree centigrade.
Soaking time               -   180 minutes.
Rate of heating            -   130 Degree centigrade.
Rate of heating            -   130 Degree centigrade.

Storage tank detail:
Shell thickness              - 18 mm
Annular plate thickness  -  20 mm
Clean out door neck       -  18 mm
Clean out door flange      -  20 mm
Material                         -  SA 516 Gr 70
Welding process            -   SMAW
Electrode                       -   E 7018 -1
Stress relieving temp      -   620 - 650 degree centigrade.  
Soaking time                 -   60 minutes.
Rate of heating              -   150 - 200 Degree centigrade.
Rate of heating              -   150 - 200 Degree centigrade

My doubt is whether the soaking time in the PQR is acceptable or I have to qualify another WPS.

Thanks in advance.
Manoj
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...