Dear MPK,
As per ASME B 31 series and different requirements are having different pup sizes.
For B 31.8 minimum 1D was the pup length (Means 1 time of dia) for other codes it may vary from 1D to 2D.
Hope it is clear for you.
Thanks and Regards................?
| Lakshman Kumar.B|Manager |Lanco Infratech Limited Plot No 1255 | Sanjeevani chowk | Mahanadi vihar | Cuttack 753004 Phone : + 91 671 2445033 | Mobile : +91 9937286851 |www.lancogroup.com Go Green|The future will thank you |
From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of mpk mpk
Sent: Thursday, January 19, 2012 9:03 AM
To: materials-welding
Subject: [MW:13507] Need to some ASME standard codes reference for Pup Pieces
Dear Experts,
Can any body Give the Minimum length of the Onshore and offshore pup piece fabrication and welding ?
Need to some ASME standard codes reference..
thank you,
MPK
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/